ORDER 3D PRINT

ATI Backs Alloyed’s 3D Printed Superalloy for Jet Engines

UK-based alloy design firm and Oxford University-spinout Alloyed has received £1 million from the UK’s Aerospace Technology Institute (ATI) Programme to help bring a new nickel superalloy closer to use in commercial jet engines. Named ABD-1000AM, the alloy is developed for additive manufacturing, and the funding will go toward resolving one of the more stubborn […]

Go to Source
Author: Paloma Duran