Researchers Develop New Tool to Control Superalloy Properties in LPBF
Researchers from the IMDEA Materials Institute have developed a new process to predict and control the microstructure of nickel-based superalloys during metal 3D printing. The team created a tool that allows manufacturers to control metal powder grain structure by adjusting parameters such as laser power, scan speed, hatch distance, and scan track length. In particular, […]