Verification of NASA superalloy opens door to next-generation 3D printed aerospace components
3D Systems, a US-based provider of solutions for additive manufacturing, has announced the successful verification of properties for GRX-810, NASA‘s new laser powder bed fusion superalloy. This innovative oxide dispersion-strengthened alloy possesses exceptional mechanical properties and temperature resistance, making it ideal for aerospace applications. The NASA-developed GRX-810 metal 3D printing material has the potential to […]
Go to Source